WokStation

Depressed that I'm gonna have to send my cool plate supertack back.

When it actually stuck, the finish was glorious, but it's simply not reliable even with scrubbing it clean with hot soapy water, leveling it, and adding hefty brims.

Any recommendations for a smooth plate for pla, silk pla and occasional petg, for a p1s?

They replied to the return request, said "as its a no reason return, you have to bear the cost of postage"!
It's a fault return, it doesn't work as advertised.

@wokstation Bambu's Cool Plate Supertack has been a big disappointing for me too. On the other hand, I've had excellent results with their standard “Smooth PEI Plate” in my P1S for PLA and PETG. Be sure and use a glue on the Smooth PEI plate when printing PETG. Bambu's liquid glue works well, is easy to apply, and easy to remove using dish soap and water.

@AA7US sounds good, I'll check into it! Thanks 👍